Learn more about ExtremeHeatSeal a crack or leaking seam in a cast iron wood stove, firebox or grill body with J-B Weld ExtremeHeat, a metallic paste rated to 1000°F. With the stove cold, wire-brush the crack, work the paste in and let it set 2 to 4 hours. Let it cure 24 hours and keep water off it, then light a small fire first. Keep it out of direct flame and off any surface that touches food.
- Difficulty
- Moderate
- Working time
- 45 min
- Cure time
- Sets in 2-4 hr, full cure 24 hr
- Works on
- Cast ironSteel
How to fix a crack in a cast iron wood stove or grill
-
Step 1: Let it cool
Let the stove or grill cool completely and clean out the ash.
-
Step 2: Prepare
Remove dirt, debris or loose contaminants from surface. Use sand paper to roughen. For some repairs, open small cracks further with a drill or screwdriver to create a 1/8" gap.
-
Step 3: Mix
Open J-B Weld® Extreme Heat™. Thoroughly mix product.
-
Step 4: Apply
Use product generously, working onto surface or into hole, crack, pit or seam. Repeat as needed. Allow 2-4 hours set up, depending on temperature and current environment.
-
Step 5: Dry
Test cure by pressing fingernail or thumbnail into repair material. If unable to penetrate, then repair is complete. If area appears slightly soft, use a non-flame heat source, such as a hair dryer, to speed cure time, or allow 24 hours before allowing high heat exposure. Repeat test until fully cured.
-
Step 6: Break it in gently
Once fully cured, start with a small fire and check the repair before running it hot.
Frequently asked questions
Can I use ExtremeHeat to repair a cracked cast iron wood stove or firebox?
Is ExtremeHeat safe for grills, smokers, ovens or anything that touches food?
What is the maximum temperature ExtremeHeat Paste can handle?
How long does ExtremeHeat take to set and cure, and can I speed it up?
NEED HELP FINDING THE RIGHT PRODUCT FOR YOUR PROJECT